1 |
2021-10-03 00:00:00 Comment: Dismantling of existing surface completed 10
|
2021-10-03 00:00:00 Comment: Thickness of cc was checked and found 4.8"&5"instead of 6"
Expansion joints not filled with sealing compound
RG chamber depth randomly checked at site and found 420mm instead of 800mm 45%
|
2022-03-24 00:00:00 Comment: •Thin hairline cracks were observed on the laid CC surface, It needs to be rectified.
•Proper camber was not provided at some places. It needs to be rectified.
•No copy of Mix –Design M-30 d 70%
|
Comment: |